by Dmitriy Nikitin | Aug 8, 2016 | Applications
The anodized aluminum key chains were marked with the 10-watt q-switched ytterbium fiber laser. All samples marked extremely well. The cycle time for marking the words Laser Photonics was 2.75 seconds. The parts were marked using 60% power. A 160 mm focal length lens...
by Dmitriy Nikitin | Aug 8, 2016 | Applications
The anodized aluminum key chains were marked with the 10 watt q-switched ytterbium fiber laser. All samples marked extremely well. The cycle time for marking the words Laser Photonics was 2.75 seconds. The parts were marked using 60% power. A 160 mm focal length lens...
by Dmitriy Nikitin | Aug 8, 2016 | Applications
The sample was marked with a 10 watt q-switched ytterbium fiber laser with 160 mm focal length lens. The 160mm focal length lens has a working distance of 176mm from lens to part. The sample was surface annealed to create contrast mark. Painted Brass and Anodize...
by Dmitriy Nikitin | Aug 8, 2016 | Applications
The sample was marked with a 10 watt q-switched ytterbium fiber laser with 160 mm focal length lens. The 160mm focal length lens has a working distance of 176mm from lens to part. The sample was surface annealed to create contrast mark. Painted Brass and Anodize...
by Dmitriy Nikitin | Aug 8, 2016 | Applications
The sample was marked with a 10 watt q-switched ytterbium fiber laser with 160 mm focal length lens. The 160mm focal length lens has a working distance of 176mm from lens to part. The sample was surface annealed to create contrast mark. Painted Brass and Anodize...