by Dmitriy Nikitin | Aug 8, 2016 | Applications
The part was laser marked with a 20 watt q-switched ytterbium fiber laser with a 160 mm focal length lens. This sample was annealed, or surface marked, to create bright contrast between the material and the mark. This process used the laser at a setting of 16 Watts,...
by Dmitriy Nikitin | Aug 8, 2016 | Applications
The parts were marked with a 10 watt q-switched ytterbium fiber laser and 160 mm focal length lens. The 160mm focal length lens has a working distance of 176mm from lens to part. Two passes were needed to darken the steel with out causing too much warping of the...
by Dmitriy Nikitin | Aug 8, 2016 | Applications
The part was marked using a 20Watt Fiber Laser Marking System using a 160 mm lens. The cycle times for the part was below one second.
by Dmitriy Nikitin | Aug 8, 2016 | Applications
The part was marked using a 20Watt Fiber Laser Marking System using a 160 mm lens. The cycle times for the part was below one second.
by Dmitriy Nikitin | Aug 8, 2016 | Applications
The part was marked using a 20 watt q-switched ytterbium fiber laser with 160 mm focal length lens. The 160mm focal length lens has a working distance of 176mm from lens to part. The ceramic sample was marked twice, using two different sets of parameters. The first...