514

Material: Aluminum Power:      18 watts – Paint Removal      18 watt – Etching Method used: Engraving Frequency:      25 kHz – Paint Removal      80 kHz – Etching Depth:...

516

Laser Marking of the stainless steel tags was done using the 20-watt q-switched ytterbium fiber laser, along with a 160 mm focal length lens. The tags marked with an annealed surface mark. The cycle time for the mark was 28.03 seconds. The cycle time includes...

522

This sample ID Tag was marked using a 20 watt Fiber laser marking system. The tag was surface annealed, to remove the paint and create contrasting marks.

544

This part was marked using a 20 watt q-switched ytterbium fiber laser with 160 mm focal length lens. The 160mm focal length lens has a working distance of 176mm from lens to part. The part was surface annealed to create sharply contrasting marks. 16 watts of power...