by Dmitriy Nikitin | Aug 8, 2016 | Applications
Laser marking on steel
by Dmitriy Nikitin | Aug 8, 2016 | Applications
All samples were marked with the 20 Watt Fiber Laser Marking system using a 160 mm lens. Characters 0.070” tall were marked on all samples. Annealing was used to create the marks on Samples 1 and 2. The surface etching was used to mark Sample 3. Sample 2 was marked at...
by Dmitriy Nikitin | Aug 8, 2016 | Applications
Laser marking was accomplished using a 20 Watt Fiber Laser
by Dmitriy Nikitin | Aug 8, 2016 | Applications
The bearing parts were marked using a 20Watt Fiber Laser System using a 160 mm lens. The inner rings were marked with a narrow font in addition to a bold font. The narrow font had a cycle time of 4.35 seconds. The bold font had a cycle time of 6.21 seconds. In order...
by Dmitriy Nikitin | Aug 8, 2016 | Applications
Laser marked stainless steel