by Dmitriy Nikitin | Aug 8, 2016 | Applications
The parts were marked using a 20 Watt Fiber Laser using a 160 mm lens. The samples were ablated using 8 Watts of power, frequency of 80 kHz, speed of 30″ per second, resulting in a cycle time of 1 minute and 33.51 seconds for the text and 2 minutes and 23.09...
by Dmitriy Nikitin | Aug 8, 2016 | Applications
This part was marked using a 20 watt Fiber laser marking system. The part was surface annealed, to remove the black paint and create contrasting marks.
by Dmitriy Nikitin | Aug 8, 2016 | Applications
This part was marked using a 20 watt Fiber laser marking system. The part was surface annealed, to remove the black paint and create contrasting marks.
by Dmitriy Nikitin | Aug 8, 2016 | Applications
This part was marked using a 20 watt Fiber laser marking system. The part was surface annealed, to remove the black paint and create contrasting marks.
by Dmitriy Nikitin | Aug 8, 2016 | Applications
All samples were marked with the 20 Watt Fiber Laser Marking system using a 160 mm lens. Characters 0.070” tall were marked on all samples. Annealing was used to create the marks on Samples 1 and 2. The surface etching was used to mark Sample 3. Sample 2 was marked at...