by Dmitriy Nikitin | Aug 8, 2016 | Applications
This part was laser marked with a 20-watt q-switched ytterbium fiber laser with a 160 mm focal length lens. This sample was surface etched, creating a light mark on the surface of the material. This process utilized the laser at a power setting of 9 Watts, with a...
by Dmitriy Nikitin | Aug 8, 2016 | Applications
This part was marked using a 20 watt Fiber laser marking system. The part was surface annealed, to remove the black paint and create contrasting marks.
by Dmitriy Nikitin | Aug 8, 2016 | Applications
This part was marked using a 20 watt Fiber laser marking system. The part was surface annealed, to remove the black paint and create contrasting marks.
by Dmitriy Nikitin | Aug 8, 2016 | Applications
The parts were marked using a 20 Watt Fiber Laser using a 160 mm lens. The samples were ablated using 8 Watts of power, frequency of 80 kHz, speed of 30″ per second, resulting in a cycle time of 1 minute and 33.51 seconds for the text and 2 minutes and 23.09...
by Dmitriy Nikitin | Aug 8, 2016 | Applications
The part was marked using a 20 Watt Pulsed Fiber Laser using a 254 mm lens. Four passes were used to ablate the sample, 2 passes each in opposite direction. For the first 2 passes, the sample was ablated using 5 Watts of power, frequency of 80 kHz, speed of 5″...