cropped-LP-LogoSymbolOnly-Color-011723.webpMENU

698

Material:  Black Polypropylene Method Used:  Etch Depth:  <.001 Laser Type:  20 watt Q-Switch Fiber Laser Focal Length Lens:  160mm Power: 30 – 100% Frequency: 20kHz Speed: 26 – 60 inches per second Passes: 1 Cycle Time: 156 – 188ms Samples were...

699

Material:  Glass Method Used:  laser marking Depth:  Surface Laser Type:  100W CW CO2 (10.6um) Focal Length Lens:  300mm Power: 10% Frequency: 5kHz modulated Speed: 500mm/sec Passes: 5 Cycle Time:...

700

Material:  Steel Method Used:  etch Depth:  >.003 Laser Type:  20 Watt Q-Switch Fiber Laser Focal Length Lens:  160mm Power: 98% Frequency: 20 kHz Speed: 15 inches per second Passes: 20 Cycle Time: 1176 seconds Samples...

701

Material:  Plastic Method Used:  etch Depth:  <.001 Laser Type:  20 Watt Q-Switch Fiber Laser Focal Length Lens:  160mm Power: 57% Frequency: 20 kHz Speed: 20 inches per second Passes: 1 Cycle Time: 9.98 seconds Samples...

681

Material:  Steel Power:  100% Method Used:  Laser annealing Frequency:  55kHz Depth:  Surface Speed:  300mm/sec Laser Type:  Pulsed fiber laser (1064nm, 1mJ @ 20kHz) Passes: 2 Focal Length Lens:  100mm...

682

Material:  Chromed steel Power:  100% Method Used:  Laser annealing Frequency:  80kHz Depth:  Surface Speed:  600mm/sec Laser Type:  Pulsed fiber laser (1064nm, 1mJ @ 20kHz) Passes: 2 Focal Length Lens:  420mm Cycle Time:   7.8sec Sample was processed with a pulsed...