cropped-LP-LogoSymbolOnly-Color-011723.webpMENU

396

The parts were laser ablated with a 10 watt q-switched ytterbium fiber laser and 420 mm focal length lens. The 420mm focal length lens has a working area of 420mm square. The parts were surface ablated to created contrast on the samples.  

412

The sample was marked with a 20 watt Fiber Laser Marking System. This process can be repeated using anywhere from a 5 watt to a 20-watt laser. The parts were marked in 0.78 seconds. The logo was marked in 0.45 seconds and “LP” was marked in 0.33 seconds. Process...

428

The part was marked using a 20 watt q-switched ytterbium fiber laser with 160mm focal length lens. The patch was marked first, and the 2D code and text were marked on top of it. The patch was surface etched onto the material using 14 watts of power, with a frequency...

446

Material: Chrome Plate Power: 18 Watt Method used: Surface Marking Frequency: 25 kHz Depth: Surface Speed: 15, 20, 30 inch/sec Laser Type: Q-Switched Fiber Laser Focal Length Lens: 160mm Cycle Time: Varies The parts were marked with a 20Watt Fiber Laser Marking System...

466

The various HMWPE (High Molecular Weight Polyethylene) were sent in for processing with our 20 watt fiber laser. The customer’s logo was generated and lased on all the various color samples and implants using various laser parameters to achieve the best overall...