by Dmitriy Nikitin | Aug 8, 2016 | Applications
Material: Brass Power: 15 Watt Method used: Annealing Frequency: 30 kHz Depth: Surface Speed: 20 inches per second Laser Type: Q-Switched Fiber Laser Focal Length Lens: 160mm (170mm WD) Cycle Time: 6.87 Seconds The sample was marked with the 20 Watt Fiber Laser...
by Dmitriy Nikitin | Aug 8, 2016 | Applications
The UID code was made with an etched mark using a 20Watt Fiber Laser Marking System with a 160 mm lens. The 2D code and serial number were readable. The cycle time for the 2D code was 2.23 seconds and the cycle time for the serial number was 2.3 seconds. The mark...
by Dmitriy Nikitin | Aug 8, 2016 | Applications
The parts were marked with a 20-watt q-switched ytterbium fiber laser and a 160 mm focal length lens. The parts were surface etched to remove a layer of material and create a brightly contrasting mark. Process Parameters: Material: Green Ceramic Power: 14 Watts Method...
by Dmitriy Nikitin | Aug 8, 2016 | Applications
The part marked had a cycle time of 6.6 seconds. The part was marked using a 10 watt Fiber Laser Marking System.
by Dmitriy Nikitin | Aug 8, 2016 | Applications
Laser marking on steel using a fiber laser
by Dmitriy Nikitin | Aug 8, 2016 | Applications
These samples were laser marked using a fiber laser