cropped-LP-LogoSymbolOnly-Color-011723.webpMENU

638

Process Parameters: Abrasive Core Material: Darker – Etching Material: Lighter – Engraving Power: Etch: 9 Watts Power: Engrave: 10 Watts Method used: Etching & Engraving Frequency: Etch: 30kHz Frequency: Engrave: 35 kHz Depth: Surface Speed: Etch: 10...

628

The samples were marked using a 20 watt Q-switched Fiber Laser using a 160 mm lens. The Colt logo (vector graphic) was annealed using 15 Watts of power, frequency of 80 kHz, speed of 5″ per second, resulting in a cycle time of 8.65 seconds. The FBI logo (raster...

622

The parts were marked using a 20 Watt Pulsed Fiber Laser using a 420mm lens. Three trials were made. The fastest marking trial was when 12 Watts of power was used with frequency of 20 kHz and speed of 40″ per second. The cycle time for this trial was 0.61 second...

625

This anodized aluminum tube was marked with a 20 watt q-switched ytterbium fiber laser at 9 watts with a frequency of 25kHz and 160mm focal length lens. The part was surfaced etched to remove the anodized layer to create the mark. The mark was created at 30 inches per...

629

The parts were marked with a 20 watt q-switched ytterbium fiber laser and 160 mm focal length lens. Process Parameters: Material: Steel Power: 16 Watts Method used: Ablation Frequency: 80 kHz Depth: Surface Speed: 10 inch/sec Laser Type: Q-Switched Fiber Laser Focal...