by Dmitriy Nikitin | Aug 8, 2016 | Applications
Laser marked steel, accomplished using a Fiber Laser
by Dmitriy Nikitin | Aug 8, 2016 | Applications
The part was marked using a 20Watt Fiber Laser Marking System using a 160 mm lens. The part was marked with both a light etch and a dark surface mark. The light etched marks had a cycle time of 0.275 seconds and the dark surface marks had a time of 1.86 seconds. If...
by Dmitriy Nikitin | Aug 8, 2016 | Applications
Process Parameters: Black Anodize Material: Black Anodized Power: 12 Watt The method used: Etch Frequency: 30 kHz Depth: Surface Speed: 15 inch/sec Laser Type: Q-Switched Fiber Laser Focal Length Lens: 160mm Cycle Time: 3.4 seconds The parts were laser marked with a...
by Dmitriy Nikitin | Aug 8, 2016 | Applications
This part was marked using a 20 watt Fiber laser marking system. The part were surface annealed, to remove the black paint and create contrasting marks.
by Dmitriy Nikitin | Aug 8, 2016 | Applications
Marks done with a speed of 250 mm/sec were done in 59.43 seconds (15 passes). Marks done with a speed of 600 mm/sec were done in 58.91 seconds (25 passes). Technology: Q-Switched Fiber Laser Wattage: 20 Watt Wavelength: 1060nm – 1070nm Focal Length Lens: 160mm...
by Dmitriy Nikitin | Aug 8, 2016 | Applications
This titanium sample used 16 watts of power resulting in very high-quality dark marks at 5.98 (larger logo) and 4.21 (smaller logo) cycle times. Technology: Q-switched Fiber Laser, Wattage: 20 Watt Focal Length Lens: 160mm.