cropped-LP-LogoSymbolOnly-Color-011723.webpMENU

323

Process Parameters: Black Anodize Material: Chrome Power: 10 Watt Method used: Etch Frequency: 35 kHz Depth: Surface Speed: 15 inch/sec Laser Type: Q-Switched Fiber Laser Focal Length Lens: 160mm Cycle Time: 4.62 seconds The parts were laser marked with a 20 watt...

342

This part was marked using a 20 watt Fiber laser marking system. The part was surface annealed, to remove the black paint and create contrasting marks.

361

All samples were marked with the 20 Watt Fiber Laser Marking system using a 160 mm lens. Characters 0.070” tall were marked on all samples. Annealing was used to create the marks on Samples 1 and 2. Surface etching was used to mark Sample 3. Sample 2 was marked at...